Mechanical Properties Metric English Comments
Flexural Modulus 0.0414 GPa
6.00 ksi
Procedure B, 0.05 in/min; ASTM D790
S&E Specialty Polymers TufTech™ 12-041 PVC Compound
Application: A PVC based semi-rigid compound designed for general purpose use in extruded form, including piping applications.Information provided by S&E Specialty Polymers
Flexural Modulus 0.0414 GPa
6.00 ksi
ASTM D790
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Flexural Modulus 0.0414 GPa
6.00 ksi
1% secant; ASTM D790
ExxonMobil Escorene® UL 7520 Adhesive Application Resin
Escorene Ultra UL 7520 is a high flow, 18.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealan..
Flexural Modulus 0.0414 GPa
6.00 ksi
1% secant; ASTM D-790
DSM Biomedical CarboSil® 10 90A Biocompatible Silicone Polycarbonate Urethane  (discontinued **)
Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-En..