Material Notes:
Application: An olefin based insulation and jacketing compound formulated to meet the UL VW-1 Standard and CSA test C22-2 No. 0.6 flame test.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Melt Flow 1.0 - 5.0 g/10 min
1.0 - 5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength 13.1 MPa
1900 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature <= -25.0 °C
<= -13.0 °F
ASTM D746
Oxygen Index >= 27 %
>= 27 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D229
Dielectric Constant 2.4
2.4
ASTM D1531
Descriptive Properties Value Comments
200% Modulus 7.02 lb-f
ASTM D638