Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers AcryliMax 301HP ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name AcryliMax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers AcryliMax 301HP ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Heat resistant flame retardant ABS battery molding compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.17 - 1.21 g/cc
1.17 - 1.21 g/cc
ASTM D792-91
Melt Flow 6.0 - 10 g/10 min
6.0 - 10 g/10 min
ASTM D1238-95
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 42.1 MPa
>= 6100 psi
ASTM D638-97
Elongation at Break >= 10 %
>= 10 %
ASTM D638-97
Flexural Modulus >= 2.55 GPa
>= 370 ksi
ASTM D790-97
Izod Impact, Notched >= 0.801 J/cm
>= 1.50 ft-lb/in
ASTM D256-97
Gardner Impact >= 2.71 J
>= 2.00 ft-lb
ASTM D5420-96
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 98.0 °C
>= 208 °F
ASTM D648-97
Flammability Test 5.0

@Thickness 3.17 mm
5.0

@Thickness 0.125 in
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved