Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX CRN720V PPE+PA6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX CRN720V PPE+PA6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GF20% FR-GTX, Restricted to sell for new customers
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0090 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103 MPa
14900 psi
SABIC - Japan Method
Elongation at Break 10 %
10 %
SABIC - Japan Method
Flexural Strength 161 MPa
23400 psi
ASTM D790
Flexural Modulus 7.07 GPa
1030 ksi
ASTM D790
Izod Impact, Notched 0.810 J/cm
1.52 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
21.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 197 °C

@Thickness 6.40 mm
387 °F

@Thickness 0.252 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved