Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX APS430 PPE+PPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX APS430 PPE+PPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE + PPS GF 30%, FR V-0
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 43.6 g/10 min

@Load 5.00 kg,
Temperature 300 °C
43.6 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 122 MPa
17700 psi
SABIC - Japan Method
Elongation at Break 10 %
10 %
SABIC - Japan Method
Flexural Strength 166 MPa
24100 psi
ASTM D790
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.780 J/cm
1.46 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 18.0 - 58.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
10.0 - 32.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 255 °C

@Thickness 6.40 mm
491 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 3.3

@Frequency 50.0 - 60.0 Hz
3.3

@Frequency 50.0 - 60.0 Hz
ASTM D150
Users viewing this material also viewed the following: