Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D 792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.0 MPa
8850 psi
SABIC - Japan Method
Elongation at Break 220 %
220 %
SABIC - Japan Method
Flexural Strength 94.0 MPa
13600 psi
ASTM D 790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D 790
Izod Impact, Notched 7.35 J/cm

@Temperature 23.0 °C
13.8 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 133 °C

@Thickness 3.20 mm
271 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Users viewing this material also viewed the following: