Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.35 J/cm @Temperature 23.0 °C |
13.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® EBC3002 PC+ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Izod Impact, Notched | 7.35 J/cm @Temperature 23.0 °C |
13.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL5302 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Izod Impact, Notched | 7.36 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Asia Pacific) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Izod Impact, Notched | 7.35 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LCR200 PBT+PC (Asia Pacific) |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
13.8 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028.. |
|||
Izod Impact, Notched | >= 7.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.8 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000M PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide.. |
|||
Izod Impact, Notched | >= 7.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.8 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 7.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.8 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 7.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.8 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® SC-1220UR PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® SC-1220UR PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3020A Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020A is a high flow grade with heat stabilizers.Information provided by Samyang. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain.. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3020PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020PJ is a high flow grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3020U UV Stable Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020U is a high flow, UV Stable grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |
|||
Izod Impact, Notched | >= 7.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.8 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 7.35 J/cm | 13.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® MHL1110 PC (Asia Pacific) |
|||
Izod Impact, Notched | 7.35 J/cm @Thickness 3.17 mm |
13.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |