Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* MH0255A is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features include; High Specific Gravity.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 2.55 g/cc
0.0921 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 MPa
2030 psi
5 mm/min; ISO 527
Elongation at Break >= 5.0 %
>= 5.0 %
5 mm/min; ISO 527
Flexural Yield Strength 28.0 MPa
4060 psi
2 mm/min; ISO 178
Flexural Modulus 4.40 GPa
638 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Users viewing this material also viewed the following: