Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.55 g/cc | 0.0921 lb/in³ | Apparent |
Gouda Vuurvast AK 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% .. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | Apparent |
Gouda Vuurvast AK 60 AP Dense Refractory Brick Description: This phosphate bonded brick combines a very good thermal shock resistance with high slag resistance and low creep. Application: frit melting furnaces, incinerators, burner blocks, lime .. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | Apparent |
Gouda Vuurvast AK 70 M Dense Refractory Brick Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,.. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | |
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | |
Schott B270â„¢ Sheet Glass B 270â„¢ crown glass in sheet glass form. Manufactured by the up-draw method, offers high stability with respect to solarization in combination with high transmission in the visible wavelength ra.. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | |
Schott Nextrema® 712-3 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | |
SGL Carbon Group EK 305 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | |
Schott N-KZFS2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MH0255A is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features include; High Specific Gravity.This data was supplied by SABIC-IP for the Europe-.. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | ISO 1183 |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | |
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties .. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #11 Filtration Granule (Corona) 3M #11 Filtration Granules are natural minerals used for water filtration in irrigation system.Information provided by 3M |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #11 Roofing Granule (Corona) 3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #11 Roofing Granule (Little Rock) 3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #14 Roofing Granule (Corona) 3M #14 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M #18 Roofing Granule (Corona) 3M #18 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M 7000 Series Copper Roofing Granule (Little Rock) 3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treate.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Blended #11 Blended Roofing Granule (Little Rock) 3M #11 Grade Blended Roofing Granules are combination of ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Cool Roofing Granule (Corona) 3M Cool Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products and are designed specifically to have a higher total solar reflectance than standard granu.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Headlap Roofing Granule (Corona) 3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He.. |
|||
Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
3M Headlap Roofing Granule (Little Rock) 3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He.. |
|||
Density | 2.55 g/cc | 0.0921 lb/in³ | Apparent |
Gouda Vuurvast SiC 70 Dense Refractory Brick Description: This type of brick, based on silicon carbide, is because of a very good thermal shock resistance, abrasion resistance and a high thermal conductivity very well suited for waste incinera.. |