Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp IF008 PA 6/12

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp IF008 PA 6/12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* IF008 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
ASTM D 638
Flexural Strength 255 MPa
37000 psi
ASTM D 790
Flexural Modulus 10.56 GPa
1532 ksi
ASTM D 790
Izod Impact, Notched 1.01 J/cm

@Temperature 23.0 °C
1.89 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 199 °C

@Thickness 3.20 mm
390 °F

@Thickness 0.126 in
unannealed; ASTM D 648