SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* UCF26AS is a compound based on Polyphthalamide resin containing 30% Carbon Fiber, 10% Glass Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 249 MPa
36100 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 24.33 GPa
3529 ksi
50 mm/min; ASTM D638
Flexural Strength 351 MPa
50900 psi
ASTM D790
Flexural Modulus 22.75 GPa
3300 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.01 J/cm
15.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 267 °C

@Thickness 3.20 mm
513 °F

@Thickness 0.126 in
unannealed; ASTM D648