Polymer Property : Tensile Strength at Break = 36100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 249 MPa
36100 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA
LNP* THERMOCOMP* UCF26AS is a compound based on Polyphthalamide resin containing 30% Carbon Fiber, 10% Glass Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive..
Tensile Strength at Break 249 MPa
36100 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA (Asia Pacific)
LNP* Thermocomp* UCF26AS is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Heat Stabilized.