Material Notes:
LNP THERMOCOMP* RF0069S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm

@Time 86400 sec
0.010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
23900 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Flexural Strength 240 MPa
34800 psi
ASTM D790
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D4812
Users viewing this material also viewed the following: