Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP DB0049R PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP DB0049R PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* DB0049R is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
5 mm/min; ISO 527
Elongation at Yield 4.8 %
4.8 %
5 mm/min; ISO 527
Tensile Modulus 2.80 GPa
406 ksi
1 mm/min; ISO 527
Flexural Yield Strength 86.0 MPa
12500 psi
2 mm/min; ISO 178
Flexural Modulus 2.80 GPa
406 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
286 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
UL 94