Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON REF42XXP PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON REF42XXP PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* REF42XXP is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 189 MPa
27400 psi
5 mm/min; ISO 527
Elongation at Break 3.1 %
3.1 %
5 mm/min; ISO 527
Flexural Strength 250 MPa
36300 psi
2 mm/min; ISO 178
Flexural Modulus 8.70 GPa
1260 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80*10*4; ISO 180/1U
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
ASTM D257
Users viewing this material also viewed the following: