Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Lubricomp NL002 PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Acetal (POM) , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Lubricomp NL002 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* PCAL4020S is a compound based on PC+ABS Blend resin containing PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
5 mm/min; ISO 527
Elongation at Break >= 25 %
>= 25 %
5 mm/min; ISO 527
Flexural Strength 75.0 MPa
10900 psi
2 mm/min; ISO 178
Flexural Modulus 2.10 GPa
305 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 109 °C
228 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL 94