SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* RI001 is a compound based on Nylon 66 resin containing Silicone.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 57.0 MPa
8270 psi
5 mm/min; ISO 527
Tensile Strength, Yield 69.0 MPa
10000 psi
5 mm/min; ISO 527
Elongation at Break 58 %
58 %
5 mm/min; ISO 527
Elongation at Yield 23 %
23 %
5 mm/min; ISO 527
Flexural Strength 85.0 MPa
12300 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 97.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
53.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 133 µm/m-°C

@Temperature 23.0 - 60.0 °C
73.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2