Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® RCY6215 PC+ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® RCY6215 PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
Physical Properties Metric English Comments
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 260 °C
24 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 64.0 MPa
9280 psi
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.92 GPa
424 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 89.0 MPa
12900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.64 GPa
383 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 5.00 J/cm
9.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 3.20 mm
185 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525