SABIC EPS 650FF Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer SABIC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC EPS 650FF Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Fire retardant expanded Polystyrene EPS 650FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process and it contains a fire retarding additive in the formulation. EPS 650FF is an expandable polystyrene grade supplied in free-flowing beads containing pentane (CFC free) as a foaming agent.Typical Applications: EPS 650FF grade is used for articles with large shape molding block molding with medium density for thermal insulation in the construction industry. EPS 650FF has retarded ignitability and the moldings made from it will conform to the requirement of DIN 53438 class K1 and K2.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.0150 - 0.0250 g/cc
0.000542 - 0.000903 lb/in³
Normal range, one pre-expansion
Bead Size 0.900 - 1.40 mm
0.0354 - 0.0551 in