Material Notes:
Ultra Fast™ Adhesives for Wire Harness, Strain Relief, Coil Coating and TerminatingCost EffectiveUltra Light-Weld® UV/Visible adhesives set in as little as one secondOn a material cost per application basis, Ultra Light-Weld adhesives are more cost effective than tape or cyanoacrylatesUltra Light-Weld adhesives are easy to integrate on automatic winders (single and multi-spindle)Improved PerformanceStructural adhesion to all types of wire, wire cladding, bobbins, ferrites, ceramics and phenolicsBetter durability than tapes, cyanoacrylates, solvent activated adhesives, hot melts or epoxiesMaterial has better thermal resistance than cyanoacrylatesMeets Mil Std 202 (Test methods 106E and 107G)Fast, Two Step ProcessingDispense AdhesiveCure in seconds with Dymax UV lightsourceDymax 3-3095 Ultra Fast™ Tack Gel AdhesiveFastest cure available; tack-free surface in 3 seconds or less; excellent as manufacturing aid or jig; replaces tape. Cure Type: UV Typical Use: For use as temporary or permanent bonder
Processing Properties Metric English Comments
Cure Time <= 0.0167 min
<= 0.000278 hour