Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ritelok TL22 Screwlock

Category Polymer , Adhesive , Thermoset
Manufacturer Ritelok
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok TL22 Screwlock.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anaerobic. Low strength threadlocker for fasteners less than 1/4". Prevent corrosion, Vibration resistant, Dismantle using normal tools
Physical Properties Metric English Comments
Viscosity 1200 - 5000 cP
1200 - 5000 cP
Mechanical Properties Metric English Comments
Impact Test 2.26 - 5.65 J
1.67 - 4.17 ft-lb
Torque Prevail
5.65 - 11.3 J
4.17 - 8.33 ft-lb
Torque Break
Descriptive Properties Value Comments
Maximum Bolt Size 0.64 cm
Copyright © lookpolymers.com All Rights Reserved