Resin Technology Group 15 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group 15 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Technology Group 15 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Physical Properties Metric English Comments
Viscosity 2000 cP
2000 cP
Mechanical Properties Metric English Comments
Adhesive Bond Strength 28.2 MPa
4090 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Descriptive Properties Value Comments
Color Clear