Reade Advanced Materials Zirconium Silicate (Zircon) Powder (ZrSiO4)

Category Ceramic , Oxide , Silicon Oxide , Zirconium Oxide
Manufacturer Reade Advanced Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reade Advanced Materials Zirconium Silicate (Zircon) Powder (ZrSiO4).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A fine white mineral powder that is chemically inert and stable to very high temperatures. Insoluble in water, dilute acids and hot concentrate sulfuric acid. Used as a primary source for investment casting shell molds, foundry cores, metal chills, ladle brick, welding rod coatings, abrasive cleaning, and mold washes.Forms Available: -50+270 mesh, -60+200 mesh, -200 mesh and -325 meshInformation provided by Reade Advanced Materials.
Physical Properties Metric English Comments
Specific Gravity 4.50 - 4.60 g/cc
4.50 - 4.60 g/cc
Bulk Density 2.76 - 2.92 g/cc
0.0997 - 0.105 lb/in³
Molecular Weight 183.1 g/mol
183.1 g/mol
Mechanical Properties Metric English Comments
Hardness, Mohs 7.5 - 8.0
7.5 - 8.0
Thermal Properties Metric English Comments
Melting Point 2200 - 2550 °C
3990 - 4620 °F
Descriptive Properties Value Comments
Color off white