Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.50 - 4.60 g/cc | 4.50 - 4.60 g/cc | |
Reade Advanced Materials Zirconium Silicate (Zircon) Powder (ZrSiO4) Description: A fine white mineral powder that is chemically inert and stable to very high temperatures. Insoluble in water, dilute acids and hot concentrate sulfuric acid. Used as a primary source .. |