Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.80 - 4.00 g/cc | 3.80 - 4.00 g/cc | ASTM D1457-18 |
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Specific Gravity | 3.50 - 4.00 g/cc | 3.50 - 4.00 g/cc | |
Parker Chomerics CHO-BOND 1030 Conductive Silicone Gasket Adhesive Electrically conductive one-component silicone-based RTV adhesive which greatly simplifies the problem of bonding conductive silicone EMI gaskets to metal substrates. This adhesive cures on exposure.. |
|||
Specific Gravity | 3.80 - 4.00 g/cc | 3.80 - 4.00 g/cc | |
Reade Advanced Materials Strontium Sulfate Powder (Celestite) (SrSO4) Description: A mineral source of strontium and its compounds. Sometimes used to impart iridescence to glass and pottery glazes. Used as a fining agent in crystal glass.Information provided by Reade.. |
|||
Specific Gravity | 3.80 - 4.00 g/cc | 3.80 - 4.00 g/cc | ASTM D1457-18 |
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |