Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylex® P1010FRVNH Polycarbonate, Unreinforced

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylex® P1010FRVNH Polycarbonate, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.5 MPa
9500 psi
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 6.94 J/cm

@Thickness 3.17 mm
13.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
ASTM D648
Flammability, UL94 V-0
V-0
0.062 inches
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in