Pyrotek Wollite 50 Insulating Castable

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Wollite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Wollite 50 Insulating Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting complex shapes and parts.ApplicationsSecondary insulation Foam blocks Floats Spouts AdvantagesNon-wetting Does not require preheating prior to usage Low K-factor Thermal shock resistant Ceramic fiber free Non-asbestos Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.801 g/cc
0.0289 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00447 GPa

@Temperature 375 °C
0.648 ksi

@Temperature 707 °F
Compressive Strength 12.73 MPa

@Temperature 375 °C
1846 psi

@Temperature 707 °F
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
0.210 W/m-K

@Temperature 250 °C
1.46 BTU-in/hr-ft²-°F

@Temperature 482 °F
0.230 W/m-K

@Temperature 600 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1110 °F