Pyrotek R-3C Silicone Coated Rope

Category Ceramic , Glass
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek R-3C Silicone Coated Rope.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
R-3 rope with silicone coating to increase abrasion resistance and air sealing properties.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 540 °C
1000 °F