Polymer Property : CTE, linear = 3.40 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.12 µm/m-°C

@Temperature 20.0 °C
3.40 µin/in-°F

@Temperature 68.0 °F
Pyrotek Pyrocast ZC Refractory Shapes
Aggregate Base: MulliteApplicationsDoor sill Breech plug Door jamb Information provided by Pyrotek.
CTE, linear 6.12 µm/m-°C

@Temperature 20.0 °C
3.40 µin/in-°F

@Temperature 68.0 °F
SGL Carbon Group EK 203 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..