Thermal Properties Metric English Comments
Thermal Conductivity 0.0400 W/m-K

@Temperature 100 °C
0.278 BTU-in/hr-ft²-°F

@Temperature 212 °F
Pyrotek AF-8 Mineral Fiber Paper
Pyrotek's AF-8 Mineral Fiber Paper is a low shot paper used in high temperature gasketing and as an insulating parting agent between refractory and metal work. It is a soft, flexible, clean pa..
Thermal Conductivity 0.0400 W/m-K

@Temperature 240 °C
0.278 BTU-in/hr-ft²-°F

@Temperature 464 °F
Pyrotek M-12 Compressible/Insulating Boards
ApplicationsHigh temperature gaskets Furnace covers Trough lining AdvantagesLow density Good insulating ability Information provided by Pyrotek.