Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Process Technologies Inc Silicone/Metal Metal Detectable Sanitary Gasket

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Process Technologies Inc
Trade Name Silicone/Metal
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Process Technologies Inc Silicone/Metal Metal Detectable Sanitary Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone/Metal is FDA compliant. This material is very pure and has low extractables. It performs well over a wide temperature range.Information provided by Process Technologies Inc
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232.22 °C
450.00 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Descriptive Properties Value Comments
Compatibility for Chemicals Acetone
Not Recommended
Ammonia
Good
Hydrochloric Acid
Not Recommended
Hydrofluoric Acid
Not Recommended
Hydrogen Peroxide
Good
Isopropyl Alcohol
Excellent
Nitric Acid
Good
Phosphoric Acid
Good
Sodium Hydroxide
Good
Sodium Hypochlorite
Good
Steam to 400ºF (204ºC)
Not Recommended
Sulfuric Acid
Not Recommended
Copyright © lookpolymers.com All Rights Reserved