Material Notes:
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many specific potting and encapsulating applications such as modules, strain-sensitive components, transformers, and coils. All 2500 series systems exhibit excellent performance when exposed to adverse environments and temperature ranges between -55°C and +130°C.Cytec (Conap) EN-2550 Potting and Encapsulation AdhesiveSpecifically formulated to impart a flame resistance that will meet U.L. 94 V-O rating in 1/8" test sample.Passes Thermal Shock Test (10 Cycles, -65°C to 130°C)Non-Nutrient Fungus Resistance (MIL-STD-810B)Mix Ratio: 17/100 (by Weight)
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
Cured
Water Absorption 0.075 %
0.075 %
24 hours
Water Absorption at Saturation 0.00187 %
0.00187 %
30 Days
Viscosity 3000 cP

@Temperature 25.0 °C
3000 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.0058 cm/cm
0.0058 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Ultimate 26.2 MPa
3800 psi
Elongation at Break 32 %
32 %
Thermal Properties Metric English Comments
CTE, linear 165 µm/m-°C

@Temperature 20.0 °C
91.7 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.335 W/m-K
2.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 2.10e+14 ohm-cm
<= 2.10e+14 ohm-cm
Surface Resistance 6.10e+17 ohm
6.10e+17 ohm
Dielectric Constant 4.13

@Frequency 1000 Hz
4.13

@Frequency 1000 Hz
Dielectric Strength 20.9 kV/mm

@Thickness 1.59 mm
530 kV/in

@Thickness 0.0625 in
Dissipation Factor 0.034

@Frequency 1000 Hz
0.034

@Frequency 1000 Hz
Arc Resistance >= 120 sec
>= 120 sec
Processing Properties Metric English Comments
Cure Time 240 - 360 min

@Temperature 100 °C
4.00 - 6.00 hour

@Temperature 212 °F
720 - 960 min

@Temperature 60.0 °C
12.0 - 16.0 hour

@Temperature 140 °F
10080 - 14400 min

@Temperature 25.0 °C
168.0 - 240 hour

@Temperature 77.0 °F
Pot Life 35.0 - 40.0 min

@Temperature 25.0 °C
35.0 - 40.0 min

@Temperature 77.0 °F
1 lbm
Descriptive Properties Value Comments
Color Black