Process Technologies Inc BUNA-N/Metal Metal Detectable Sanitary Gasket

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Process Technologies Inc
Trade Name BUNA-N/Metal
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Process Technologies Inc BUNA-N/Metal Metal Detectable Sanitary Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BUNA-N/Metal should be considered for use with oils and animal fats. BUNA-N/Metal should be considered for use with oils and animal fats. This material is FDA compliant and has good compression set characteristics. BUNA-N/Metal does have a limited temperature range which precludes its use in many applications.Information provided by Process Technologies Inc
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.33 °C
200.0 °F
Minimum Service Temperature, Air -34.44 °C
-29.99 °F
Descriptive Properties Value Comments
Compatibility for Chemicals Acetone
Not Recommended
Ammonia
Good
Hydrochloric Acid
Not Recommended
Hydrofluoric Acid
Not Recommended
Hydrogen Peroxide
Good
Isopropyl Alcohol
Good
Nitric Acid
Not Recommended
Phosphoric Acid
Good
Sodium Hydroxide
Good
Sodium Hypochlorite
Good
Steam to 400ºF (204ºC)
Not Recommended
Sulfuric Acid
Limited