Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -34.44 °C | -29.99 °F | |
Process Technologies Inc BUNA-N Sanitary Gasket BUNA-N should be considered for use with oils and animal fats. This is a food grade and 3A approved that has good compression set characteristics. BUNA-N does have a limited temperature range which .. |
|||
Minimum Service Temperature, Air | -34.44 °C | -29.99 °F | |
Process Technologies Inc BUNA-N/Metal Metal Detectable Sanitary Gasket BUNA-N/Metal should be considered for use with oils and animal fats. BUNA-N/Metal should be considered for use with oils and animal fats. This material is FDA compliant and has good compression set .. |
|||
Minimum Service Temperature, Air | -34.44 °C | -29.99 °F | |
Process Technologies Inc EPDM Sanitary Gasket EPDM (Ethylene Propylene Diene Monomer) This material is USP Class VI, FDA and 3A compliant. EPDM has very good water and steam resistance. Because of its polymer structure, this material does not o.. |
|||
Minimum Service Temperature, Air | -34.44 °C | -29.99 °F | |
Process Technologies Inc EPDM/Metal Metal Detectable Sanitary Gasket EPDM/Metal (Ethylene Propylene Diene Monomer) This material is FDA compliant. EPDM/Metal has very good water and steam resistance. Because of its polymer structure, this material does not offer stro.. |