Precision Polymer Engineering V72G Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V72G Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Green Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperatures. Accepted by the MOD to Defence Standard 02-337 Part 1. Issue 1 (NES 337)
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
°IRHD; ASTM D1415
71
71
°IRHD, +2 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 12.672 MPa
1837.9 psi
-1% change after 72 hours @ 250°C; ASTM D412
12.8 MPa
1860 psi
ASTM D412
Elongation at Break 140.8 %
140.8 %
-12% change after 72 hours @ 250°C; ASTM D412
160 %
160 %
ASTM D412
Compression Set 10 %
10 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Descriptive Properties Value Comments
Low Temperature Flexibility, °C -17