Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.672 MPa | 1837.9 psi | -1% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering V72G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperatures. Acc.. |