Material Notes:
Description/Features:High Performance Thermoplastic ElastomerOver-Molding GradeTransparentMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.0269 cm/cm
0.0269 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 41
41
Instant; ASTM D2240
Tensile Strength, Yield 6.89 MPa
1000 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.55 MPa

@Strain 300 %
370 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 800 %
800 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 29.8 kN/m
170 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 22 %
22 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified