Material Notes:
Description/Features:Flame RetardantMulti-Purpose Thermoplastic ElastomerApplications:General PurposeInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage 0.0127 cm/cm
0.0127 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 32
32
Instant; ASTM D2240
Tensile Strength, Yield 2.76 MPa
400 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.07 MPa

@Strain 300 %
300 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 400 %
400 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 17.5 kN/m
100 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 20 %
20 %
Method B, 73°F(23°C), 22 hrs; ASTM D395