Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0127 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0127 cm/cm
0.0127 in/in
STN 64 0808
Plastcom SLOVALEN PC 59 GF 13 Compounded Polypropylene Homopolymer, 13% Chemically Coupled Glass Fiber
FeaturesCompounded homopolymer PP, with the content of 13% chemically coupled glass fiber and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all indus..
Linear Mold Shrinkage 0.0127 cm/cm
0.0127 in/in
STN 64 0808
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C...
Linear Mold Shrinkage 0.0127 cm/cm
0.0127 in/in
Plastcom SLOVAMID 6 GF 5 PA6, 5% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 5% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
Linear Mold Shrinkage 0.0127 cm/cm
0.0127 in/in
ASTM D955
PolyOne Synprene® IT 086LFR Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Flame RetardantMulti-Purpose Thermoplastic ElastomerApplications:General PurposeInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Co..
Copyright © lookpolymers.com All Rights Reserved