Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Stat-Tech™ PF-NX-062100-2 Polysulfone  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ PF-NX-062100-2 Polysulfone  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Electrically ConductiveESD ProtectionInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.463 g/cc
1.463 g/cc
ASTM D792
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 57.9 MPa
8400 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 1.25 %
1.25 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 8.646 GPa
1254 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 93.941 MPa
13625 psi
ASTM D790
Flexural Modulus 6.45 GPa
935 ksi
ASTM D790
Izod Impact, Notched 0.366 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.686 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 800000 ohm-cm
800000 ohm-cm
ASTM D257