Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 57.9 MPa
8400 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Stat-Tech™ PF-NX-062100-2 Polysulfone  (discontinued **)
Description/Features:Electrically ConductiveESD ProtectionInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 57.9 - 57.9 MPa

@Temperature 150 - 150 °C
8400 - 8400 psi

@Temperature 302 - 302 °F
Average value: 57.9 MPa Grade Count:1
Overview of materials for Thermoplastic Polyimide, Unfilled
Tensile Strength, Ultimate 57.9 MPa

@Temperature 150 °C
8400 psi

@Temperature 302 °F
ASTM D638
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Tensile Strength, Ultimate 57.9 MPa
8400 psi
ASTM D638
Plenco 2424 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical ..
Tensile Strength, Ultimate 57.9 MPa
8390 psi
ASTM D412
SK Chemicals SKYTHANE® 155D S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 57.9 MPa
8390 psi
ASTM D412
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 57.9 MPa
8400 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 8600-10 Polycarbonate
EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental ..
Tensile Strength, Ultimate 57.9 MPa
8400 psi
ASTM D412; ASTM D638
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
Tensile Strength, Ultimate 57.9 MPa
8400 psi
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by  AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade el..