Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black
Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural
Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ATM D955
Plenco 50015 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu..
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
PolyOne Stat-Tech™ PF-NX-062100-2 Polysulfone  (discontinued **)
Description/Features:Electrically ConductiveESD ProtectionInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
Haysite 18600 Polyester BMC, 15% Glass Reinforced
The 18600 series bulk molding compound can be compression, transfer, or injection molded. Formulated with a high temperature resin system, this grade exhibits exceptional retention of physical and e..
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
Plenco 6990 Phenolic, Briquette, Transfer Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
Injection Molding; ISO 2577
Vyncolit X620/1 Novolac Phenolic
Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir..
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ASTM D955
Plenco 6401 Phenolic, Briquette, Injection Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Linear Mold Shrinkage 0.0022 - 0.0042 cm/cm
0.0022 - 0.0042 in/in
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester
BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig..
Linear Mold Shrinkage 0.0022 - 0.0040 cm/cm
0.0022 - 0.0040 in/in
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester
BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in ..
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
Polyram Polytron A40B01 Nylon 66, 40% Long Fiber
A 40% long fiber glass reinforced black nylon 6.6 heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber
A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.