PolyOne Geon™ Vinyl Flexible R323AE Polyvinyl Chloride Elastomer (PVC Elastomer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible R323AE Polyvinyl Chloride Elastomer (PVC Elastomer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
15 sec; ASTM D2240
Tensile Strength at Break 16.5 MPa
2390 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 400 %
400 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -48.9 °C
-56.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 171 - 182 °C
340 - 360 °F
188 - 199 °C
370 - 390 °F
Descriptive Properties Value Comments
Additive Biocide
Features Good Adhesion
Forms Pellets
Generic Material PVC Elastomer
Generic Name Polyvinyl Chloride Elastomer (PVC Elastomer)
Processing Method Coextrusion
Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications