Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Geon® 137 is a carboxyl functional copolymer dispersion resin providing extra adhesion to synthetic fabrics, such as nylon, allowing the elimination of adhesion promoters. It provides the ability to crosslink with epoxies, providing a more solvent resistant coating. The polarity of Geon® 137 allows its use in hydrosols. Geon® 137 is recommended for applications where special characteristics are requires, such as nylon fabric coating, hydrosol inks and coatings, solvent resistant coatings, and automotive sealants.Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 137, 77phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390(formulation): 100phr Geon® 137, and 60phr DOPInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
Bulk Density 0.400 g/cc
0.0145 lb/in³
Fineness 3.0
3.0
Hegman, North Fineness; Geon® 390
Relative Viscosity 2.55 cP
2.55 cP
Correlation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 16.3 cP
16.3 cP
Initial Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
17.9 cP
17.9 cP
One Day Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
27 cP
27 cP
Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method
32.3 cP
32.3 cP
One Day Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method
Viscosity Measurement 1.1
1.1
Inherent; ASTM D1243-60-A
Melt Flow 12 g/10 min

@Pressure 0.655 MPa
12 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
Mechanical Properties Metric English Comments
Tensile Strength 14.8 MPa
2150 psi
Optimum; With provided formulation; ASTM D638
Optical Properties Metric English Comments
Gloss 55 %
55 %
60 Degree Fused 5 mins @ 350FGeon® ALTC 65 (with provided formulation); Internal Method
Transmission, Visible 78 %
78 %
Geon® ALTC 66 (with provided formulation); Internal Method
Processing Properties Metric English Comments
Moisture Content 0.12 %
0.12 %
Karl FisherGeon® STP 683; Internal Method
Descriptive Properties Value Comments
Features Good Adhesion
Solvent Resistant
Fixed Acid 2.4%
Internal Method; Geon® STP 1315
Forms Powder
Fine, White Powder
Free Acid 0.4%
Internal Method; Geon® STP 1315
Gel Temperature 67 °C
Internal Method; Geon® ALTC 29 (with provided formulation)
Generic Material PVC Copolymer
Generic Name Polyvinyl Chloride Copolymer (PVC Copolymer)
K-Value 73
Internal Method; Correlation, 0.5gm/100ml
Methanol Extractables 3.1%
Internal Method; Geon® STP 894
Polymerization Process Microsuspension
Processing Method Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Residual Vinyl Chloride Monomer < 9 ppm
Internal Method; Geon® STP 1005
Uses Automotive Applications
Coating Applications
Fabric Coatings
Sealants
Users viewing this material also viewed the following: