Polymer Property : Brookfield Viscosity = 16.3 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 16.3 cP
16.3 cP
Initial Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
PolyOne Geon™ 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® 137 is a carboxyl functional copolymer dispersion resin providing extra adhesion to synthetic fabrics, such as nylon, allowing the elimination of adhesion promoters. It provides the ability t..