PolyOne Elastamax™ XL 0131-61 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ XL 0131-61 Styrene Butadiene Block Copolymer (SBC)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods. All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. For More Information contact PolyOne.
Physical Properties Metric English Comments
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 45

@Time 5.00 sec
45

@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 19.3 MPa
2800 psi
510 mm/min; ASTM D412A
Tensile Strength, Yield 10.5 MPa

@Strain 100 %
1520 psi

@Strain 100 %
510 mm/min; ASTM D412A
11.4 MPa

@Strain 300 %
1650 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 610 %
610 %
510 mm/min; ASTM D412A
Tear Strength 78.8 kN/m
450 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Opaque
Features Food Contact Acceptable
General Purpose
Forms Pellets
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Consumer Applications
General Purpose
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved