Physical Properties Metric English Comments
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
PolyOne Maxxam™ FR PP 301 S Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne reFlex™ 300 Plasticizer, Bio-derived
Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 99% biobased.Information provided by PolyOne
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne Synplast™ DOP-N Di (2-ethylhexyl) Phthalate
Branched C8 phthalate esterInformation provided by PolyOne
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne Synplast™ NOTM-E Tri (n-octyl) Trimellitate
Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Specific Gravity 0.978 - 0.984 g/cc

@Temperature 25.0 °C
0.978 - 0.984 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne Synplast™ NOTM-PPC Tri (n-octyl) Trimellitate
CPSIA HR 4040 Compliant Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav..
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
PolyOne Maxxam™ FR PP 301 Black 1284-11 S Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
PolyOne Maxxam™ FR PE 112 LDPE  (discontinued **)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
PolyOne Elastamax™ XL 0131-61 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco..
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
PolyOne Elastamax™ XL-0153-79 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco..
Specific Gravity 0.978 g/cc
0.978 g/cc
Teknor Apex TruVis Esters™ 810TM N-C8C10 Trimellitate
Specific Gravity 0.978 g/cc
0.978 g/cc
ASTM D792
PolyOne Elastamax™ XL-0153-24 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)