PolyMirae Moplen EP300C Sheet and Thermoforming Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen EP300C Sheet and Thermoforming Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP300C is the polypropylene blockpolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300C is a block copolymer particularly suitable for sheet and thermoforming. Moplen EP300C resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Excellent processability and stretchability; High stiffness; High mechanical properties; High melt strengthApplications: Food packaging and tray; Rigid sheet; Corrugated board; Irrigation tapeInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.08 GPa
156 ksi
ASTM D790
Izod Impact, Notched 0.588 J/cm

@Temperature -20.0 °C
1.10 ft-lb/in

@Temperature -4.00 °F
ASTM D256
6.86 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 152 °C
306 °F
ASTM D1525