Plenco 50335 PET, Pellet, Injection Molded, Black  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50335 PET, Pellet, Injection Molded, Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0019 cm/cm
0.0019 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115.4 MPa
16740 psi
ASTM D638
Elongation at Break 1.72 %
1.72 %
ASTM D638
Tensile Modulus 9.42 GPa
1370 ksi
ASTM D638
Flexural Yield Strength 171.6 MPa
24890 psi
ASTM D790
Flexural Modulus 9.06 GPa
1310 ksi
ASTM D790
Compressive Yield Strength 170.4 MPa
24710 psi
ASTM D695
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Comparative Tracking Index 175 V
175 V
ASTM D3638