Material Notes:
These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Melt Flow 14 g/10 min
14 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM 638
Elongation at Break 18 %
18 %
ASTM D638
Flexural Yield Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
0.25 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
0.25 inch; ASTM D648
UL RTI, Electrical 140 °C
284 °F
UL746B
UL RTI, Mechanical with Impact 85.0 °C
185 °F
UL746B
UL RTI, Mechanical without Impact 125 °C
257 °F
UL746B
Flammability, UL94 V-0

@Thickness 1.20 mm
V-0

@Thickness 0.0472 in